War-ships: A Text-book on the Construction, Protection, Stability, Turning, Etc., of War VesselsLongmans, Green, 1904 - 304 páginas |
Dentro del libro
Resultados 1-5 de 66
Página 1
... connection with this fore - and - aft bending and the proper arrangement of the material to make the ship strong enough , we shall first consider some properties of beams . Beams . If we take a plank , say 12 in . wide and 2 in . thick ...
... connection with this fore - and - aft bending and the proper arrangement of the material to make the ship strong enough , we shall first consider some properties of beams . Beams . If we take a plank , say 12 in . wide and 2 in . thick ...
Página 7
... connection with the scantlings adopted in a ship is the subsequent maintenance . Inspection and care of the structure of war - ships is carried out in a most careful and thorough manner , and in this way the margin for deterioration may ...
... connection with the scantlings adopted in a ship is the subsequent maintenance . Inspection and care of the structure of war - ships is carried out in a most careful and thorough manner , and in this way the margin for deterioration may ...
Página 15
... connection is established between them . For such ships , there- fore , the stem , sternpost , etc. , are made of the copper alloy , phosphor bronze . This consists of 90 per cent . copper with 10 per cent . of phosphor tin ( containing ...
... connection is established between them . For such ships , there- fore , the stem , sternpost , etc. , are made of the copper alloy , phosphor bronze . This consists of 90 per cent . copper with 10 per cent . of phosphor tin ( containing ...
Página 15
... connection is established between them . For such ships , there- fore , the stem , sternpost , etc. , are made of the copper alloy , phosphor bronze . This consists of 90 per cent . copper with 10 per cent . of phosphor tin ( containing ...
... connection is established between them . For such ships , there- fore , the stem , sternpost , etc. , are made of the copper alloy , phosphor bronze . This consists of 90 per cent . copper with 10 per cent . of phosphor tin ( containing ...
Página 16
... connection . The half round ( 1 ) is usually hollow , and is used as a moulding round the ship . The segmental bar ( m ) is used as a finish round the top of hatch coamings , etc. The sections shown in Fig . 8 are drawn to scale , and ...
... connection . The half round ( 1 ) is usually hollow , and is used as a moulding round the ship . The segmental bar ( m ) is used as a finish round the top of hatch coamings , etc. The sections shown in Fig . 8 are drawn to scale , and ...
Otras ediciones - Ver todas
Términos y frases comunes
angle armour B.Sc barbettes battle-ship beam bilge boiler-room boilers bolts bulkhead buoyancy centre change of trim CHAPTER CHEMICAL CHEMISTRY class cruiser coal coal-bunker cofferdam College compartment copper Crown 8vo curve of stability D.Sc destroyers Diagrams diameter displacement double bottom Downton pumps draught ELEMENTARY engine engine-room fitted floating flooding fore-and-aft forward framing guns heel Illustrations inner bottom INORGANIC knots length Lond longitudinal lower bunkers main deck metacentric height MIDDLE DECK moment of inertia necessary obtained outer bottom plating Owens College Ph.D phosphor bronze PRACTICAL Professor protective deck pumps recent ships resistance rivets Royal Navy Royal Sovereign rudder Scientific Works published screw sheathed ship's shown in Fig side space speed steam steel steering gear stern sternpost stiffened strake strength structure SVANTE ARRHENIUS teak thick tons per inch upper bunkers upper deck valve ventilation vessel war-ships waterline waterplane wave weight Woodcuts zed bar